Extrusion & nibbling
What you see — Seal edge is chewed or extruded into the clearance gap; usually pressure + gap + soft compound.
Reduce clearance · add back-up ring · raise compound hardness
An industry name tells you where a component works. It does not tell you why it failed. Describe the duty, identify the failure mode, then let the material and geometry follow.
Bring these six values to the conversation. Everything downstream depends on them.
Each path below is drawn from our engineering library — not from a product catalogue.
What you see — Seal edge is chewed or extruded into the clearance gap; usually pressure + gap + soft compound.
What you see — Volume gain, softening or loss of strength after exposure to an incompatible medium.
What you see — Seal no longer springs back; sealing force decays after a long hot static duty.
What you see — Surface crazing, hardening and cracks after sustained exposure above the compound rating.
What you see — Cuts, twists or nicks introduced during fitting — the largest share of early-life failures.
What you see — Blistering and internal rupture when a gas-saturated elastomer is depressurised quickly.
Industry pages remain available as a secondary index.
Include temperature, pressure, media, motion, cleanliness and target life. We reply with a material and geometry recommendation.